Pitting corrosion model for reinforced concrete structures in a chloride environment

Research output: Contribution to journalArticlepeer-review

89 Citations (Scopus)

Fingerprint

Dive into the research topics of 'Pitting corrosion model for reinforced concrete structures in a chloride environment'. Together they form a unique fingerprint.

Engineering

Material Science