Abstract
This study examines the effect of retrogression and reaging (RRA) holding time on the microstructure and corrosion behavior of Al-Zn-Mg sacrificial anodes. The process involved solution heat treatment at 470°C for 1 hour, pre-Aging at 120°C for 24 hours, retrogression at 180°C for 10, 30, and 60 minutes, and reaging at 120°C for 24 hours. Tests included Optical Emission Spectroscopy (OES), anode consumption rate, potentiodynamic polarization, EIS, XRD, hardness, and metallography, with seawater analyzed for pH, salinity, and anions. Results showed that longer retrogression times increased the size of stable η (MgZn2) precipitates and dispersed metastable η' precipitates, enhancing corrosion resistance. Copper dissolution within precipitates raised cell potential and initiated pits. The optimal holding time was 30 minutes, minimizing anode consumption and corrosion rates, while longer times caused significant increases. Passive layer thickness (Al2O3 ), inferred from CPEpass-T values, ranked as follows: 30 minutes >10 minutes >untreated >60 minutes.
| Original language | English |
|---|---|
| Article number | 060008 |
| Journal | AIP Conference Proceedings |
| Volume | 3443 |
| Issue number | 1 |
| DOIs | |
| Publication status | Published - 13 Aug 2026 |
| Event | 6th International Conference on Materials and Metallurgical Engineering and Technology, ICOMMET 2024 - Surabaya, India Duration: 12 Oct 2024 → 13 Oct 2024 |
Keywords
- Aluminum
- Cerium
- Corrosion
- Efficiency
- Sacrificial Anode
Fingerprint
Dive into the research topics of 'The effect of holding time variation in the retrogression and reaging process on the corrosion behavior of Al-Zn Mg anode for sepat 5 ship at PT. Pertamina trans Kontinental'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver